Firing is divided into 5 steps in total, and the specific steps are as follows.
Step 1. Select the mud and take the mud
It is necessary to use old loess, which should be sun-dried and thoroughly sun-dried, and there should be no miscellaneous soil.
Step 2. Stir
Saturate the loess with water, use the foot pedal, stir, and mature the mud into a ball. The loess needs to be sticky and strong.
Step 3. Making the mud
Use the turntable to turn first, then take the soil in the center of the turntable and make it into a Pot shape by hand.
Step 4. Sun dry
The pottery clay painting pot blank is ready, and it should be dried in the sun without cracks.
Step 5. Setting up the kiln and firing
The pot blanks are installed in the kiln. Burn with grass. The fire temperature in the kiln is controlled at about 1000 degrees, and it takes about 5 hours for one kiln to burn (about 60 hours for grass burning and coal burning).
Previous: How to clean terracotta pots?
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.